Altec Recalls Aerial Devices Due to Potential Weld Cracks

A cracked weld may allow the auger bracket to detach from the boom, increasing the risk of injury.

Altec Recalls Aerial Devices Due to Potential Weld Cracks

Altec will inspect and repair cracks found in the base boom, free of charge.

Photo: Altec

1 min to read


Altec Industries, Inc. (Altec) announced it is recalling approximately 975 2015-2022 DT65 and DT85 Aerial Devices, as the weld between the base boom and the auger stow bracket could crack.

Ad Loading...

A cracked weld may allow the auger bracket to detach from the boom, increasing the risk of injury.

Ad Loading...

Altec will inspect and repair cracks found in the base boom, free of charge. Owner notification letters are expected to be mailed October 7, 2022.

Altec's number for this recall is CSN-3017.

More Safety & Compliance

Work Truck graphic with “Fall Back” and “Keep Fleet Safety in Focus” over a sunlit field, with a clock illustration on the right.
Safety & Compliance•by Lauren Fletcher•October 30, 2026

Navigating the Effects of Daylight Saving Time on Work Truck Fleets

Discover how daylight saving time impacts work truck fleets and get essential tips for fleet managers and drivers to navigate the "fall back" transition.

Read More →
Three glowing jack-o’-lanterns beneath a full moon, with silhouetted trees and gravestones. Text reads “Keeping Your Drivers Safe?” above the Work Truck logo.
Safety & Compliance•by Lauren Fletcher•October 29, 2026

How Halloween Changes the Job for Work Truck Drivers

Truck traffic doesn’t take the same Halloween break as other drivers. What fleet managers should know about timing, neighborhood stops, and braking data.

Read More →
Safe Driving on Halloween over spooky fall road
Safety & Compliance•by Staff•October 25, 2026

Tips for Driving Safely on Halloween Night

This video features a reminder from the Connecticut Department of Transportation (DOT) and the Connecticut Police Chiefs Association, urging drivers to prioritize safety this Halloween.

Read More →
Ad Loading...
Work Truck graphic with a truck engine and the text “Rerating GVWR — What Fleets Need to Know.”
Safety & Compliance•by Staff•October 22, 2026

Re-rating Gross Vehicle Weight Ratings (GVWR): Why and How it's Done

Sometimes, it is not in a fleet’s best interests to have a vehicle at a given GVWR. Changing the GVWR to a special value can be done, but the process is complicated.

Read More →
Work gloves, a hard hat, tablet, keys, and paperwork sit on a workbench beside a calendar marked “Out of Service,” illustrating the operational disruption caused by a missing work truck.
Safety & Compliance•October 22, 2026

When a Work Truck Gets Stolen, the Real Loss Is Time

A stolen work truck can take more than a vehicle off the road. From tools and access cards to crew downtime, here’s how fleets can prepare for theft before it disrupts the entire workday.

Read More →
Ten members of the America's Road Team pose in front of a white Volvo semi-truck featuring patriotic graphics and the America's Road Team logo at the MCE26 conference and exhibition.
Safety & Compliance•by News/Media Release•October 21, 2026

Volvo Trucks Marks 25 Years as Exclusive Sponsor of America's Road Team

Volvo Trucks North America will serve as the exclusive sponsor of the American Trucking Associations' America's Road Team, marking 25 years of Volvo sponsorship. The group of professional drivers promotes safety and the industry as they travel the country.

Read More →
Ad Loading...
Streamlight Portable Scene Light III displayed on a tripod with a close-up of its LED light head, alongside a badge recognizing it as the 2026 OH&S New Product of the Year winner.
Safety & Compliance•by News/Media Release•October 21, 2026

Streamlight’s High-Output Scene Light Recognized with Occupational Safety Award

Streamlight’s Portable Scene Light III (PSL III) won the 2026 Occupational Health & Safety (OH&S) New Product of the Year Award in the Lighting category.

Read More →
Fleetworthy Expedited Inspection graphic featuring a commercial vehicle inspector walking toward a white semi-truck, with tablet and smartphone displays showing digital driver vehicle examination reports.
Safety & Compliance•by News/Media Release•October 14, 2026

Fleetworthy Expands Expedited Inspection to 5 States

Following its industry-first launch in Nevada, Fleetworthy’s automated inspection technology is now live in California, Michigan, Vermont, and Maine.

Read More →
Red and Black Promo graphic with Kathy Close of JJ Keller that says Behind the Article, Under 26,001 lbs.? IRP May still apply.
Safety & Compliance•by Lauren Fletcher•October 12, 2026

Crossing State Lines in a Light-Duty Work Truck? Check These Rules First

Crossing state lines in a lighter work truck? J.J. Keller's Kathy Close explains when IRP registration, trip permits, and towing rules come into play.

Read More →
Ad Loading...
Safety & Compliance•by Staff•October 12, 2026

Simple Tire Checks That Help Keep Your Business Fleet Moving

A survey found that nearly one in every 10 passenger vehicles has at least one bald tire. What's more, 27% -- more than one in four -- of vehicles are driven with one or more severely under-inflated tires.

Read More →